ERNiCrMo-2/UNS N06002/W.Nr.2.4856 AWS A5.14/ASME SFA A5.14

  • Place of Origin Jiangsu,China
  • Model Number ERNiCrMo-2
  • Trade Names UNS N06002/W.Nr.2.4856,Hastelloy X
  • Dimensions 0.8MM / 1.0MM / 1.2MM / 1.6MM / 2.4MM / 3.2MM / 3.8MM / 4.0MM / 5.0MM.Customized Size
  • Delivery Conditions Pickling, Bright
  • Avaliable Package Form MIG(15kg/spool), TIG(5kg/box), Coil
  • MOQ 15~200 (KG)
  • Production Standards AWS A5.14/ASME SFA A5.14
  • Packaging Details Wooden Case, or as per Client's request
  • Payment Terms L/C, T/T, Western Union, MoneyGram
  • Trade Terms FOB, CIF, DUP, EXW
  • Delivery Time 7~45 days

Overview


Hastelloy X filler metal is used for the gas metal arc and gas tungsten arc welding of X alloy. The deposited weld metal has an exceptional combination of oxidation resistance, fabricability and high-temperature strength. It has also been found to be exceptionally resistant to stress-corrosion cracking in petrochemical applications. X alloy exhibits good ductility after prolonged exposure at temperatures of 1200, 1400, 1600°F (650, 760 and 870°℃) for 16,000 hours. The filler metal is also a good candidate for dissimilar welding between solid solution nickel based alloys and Ni-Fe-Cr alloys. The RTWM finish on the spooled wire promotes smooth feeding through welding equipment and reduced tip wear in contact tips.


Alloy X is a nickel-chromium-molybdenum “superalloy” used for MIG, TIG or plasma arc welding of similar base metals such as Hastelloy X to itself or to stainless steel, carbon steel and low alloy steels. This filler metal offers an exceptional combination of oxidation, corrosion and thermal shock resistance. The weld deposits of Alloy X exhibit high temperature strength and resists weld metal fatigue at temperatures up to 2200°F. Alloy X is commonly used in the aerospace industry for engine tailpipes, turbine blades, nozzle vanes and after burner components. It is also used in petrochemical applications to combat stress corrosion cracking.



Limiting Chemical Composition, %


Nickel.....................................................................................................................................................................................44.00 min.

Chromium...........................................................................................................................................................................20.50-23.00

Molybdenum.........................................................................................................................................................................8.00-10.00

Manganese.............................................................................................................................................................................1.00 max.

Iron..........................................................................................................................................................................................17.0-20.0

Silicon......................................................................................................................................................................................0.10 max.

Copper.....................................................................................................................................................................................0.50 max.

Carbon.....................................................................................................................................................................................0.05-0.15

Phosphorous...........................................................................................................................................................................0.02 max.

Sulfur.....................................................................................................................................................................................0.015 max.

Tungsten..................................................................................................................................................................................0.20-1.00

Cobalt.......................................................................................................................................................................................0.50-2.50



Mechanical Properties


ErNiCrMo-2’s mechanical properties are at the heart of its appeal in welding applications, particularly in environments characterized by extreme temperatures and corrosive substances.



Tensile Properties


Tensile strength Rm (MPa)

Elongation A %

min 600

-



Corrosion Resistance


Corrosion can be a significant threat in various industrial environments. ErNiCrMo-2 boasts remarkable corrosion resistance, offering longevity and reliability even in highly corrosive conditions. This property is crucial in marine and chemical processing applications.



Product Forms And Packaging (0ther sizes available -please contact us)

 

Product

Diameter

Length

Packaging

Wire For MIG/GMAW Welding

0.8mm/1.0mm/1.2mm/1.6mm/2.0mm/2.4mm /2.5mm/3.2mm

-

33 lbs (15kgs)

Rods For TIG/GTAW Welding

2.0mm /2.4mm /2.5mm/3.2mm/4.0mm/5.0mm

915mm-1000mm

11 lbs (5kgs)

Wire For SAW Welding

2.0mm /2.4mm /2.5mm /3.2mm /4.0mm/5.0mm

-

60 lbs (27kgs)